METHOD TO MAKE ELASTIC SHIRTING FABRIC COMPRISING SPANDEX AND HARD YARN
摘要
<p>Methods for making stretch shirting fabric having fabric weight less than 175 g/m<SUP>2</SUP> and fabric stretch between 15% to 45% in the weft direction are disclosed. A corespun composite elastomeric yarn is produced either (a) by low draft (2.7 x or below) core-spinning of the elastomeric yarn, or (b) by pretreating the corespun composite yarn in steam or heated water at temperatures of at least 110°C to reduce yarn power before dyeing or weaving. The shirting fabric with such corespun composite elastomeric yarn in the weft meets end-use specifications without heat-setting.</p>