摘要 |
The component consists of a molding (2,2') of metal or plastics, with at least two overlying openings (3,3') connected together by a rivet joint (4) made of injected thermoplastics. The rivet head (4) includes a weak point (5), such as a continuous notch or groove along the diameter of the head. |