发明名称 High carbon steel wire with bainitic structure for spring and other cold-formed applications
摘要 According to the present invention, there is disclosed a heat treated high carbon or alloy steel wire and method of heat-treating the wire. The wire is produced by the steps of initially heating the high carbon or alloy steel wire to a temperature of about 1600 degrees F. to about 1800 degrees F. for between 10 seconds and 2 minutes; rapidly cooling the wire to an intermediate point temperature of between 400 to about 1000 degrees F.; holding the wire at the intermediate point temperature for about 2 minutes to about 40 minutes; and cooling the resulting wire to ambient temperature.