摘要 |
<p>A process for production of a polyolefin-based composite material of high rigidity, containing a polyolefin and a layered clay, involves impregnating a layered, swellable clay which is interstratified with a tetraalkyl cation, with at least one polymerizable monomer and then mixing this impregnated clay with a polyolefin and a peroxide, at a temperature above the melting point of the polyolefin. A polyolefin-based composite material containing 98-50 wt. % of a polyolefin, 1-50 wt. % of another homo- or copolymer and 1-50 wt. % of a layered clay, wherein the ratio between the modulus of elasticity of the material and that of the initial polyolefin, at a temperature which is 30° C. below the melting temperature of the polyolefin, is higher than or equal to 1 has high rigidity.</p> |