摘要 |
<P>PROBLEM TO BE SOLVED: To provide ceramic slurry which undergoes a reduced viscosity increase when the constituent binder is added during its preparation and has a stable ceramic concentration and stable slurry viscosity and to provide a method for producing the same. <P>SOLUTION: The method for producing the ceramic slurry is one for producing ceramic slurry comprising a ceramic powder, a solvent, and a binder, wherein at least part of the binder is added in the form of a solid powder to a mixture solution containing at least the ceramic powder and the solvent. <P>COPYRIGHT: (C)2006,JPO&NCIPI |