发明名称 MOLDING METHOD OF SLEEVE FOR PIPE JOINT
摘要 PROBLEM TO BE SOLVED: To provide the molding method of a sleeve for pipe joint that can pour the resin well in balance into a molding metal flask and bury the reinforced ring finely while maintaining the positioning. SOLUTION: A core pin 22 having a small diameter part 22a to form a thin part, an uneven part, a thick part and an inside circumference face of the sleeve, an uneven molding face 22b and a large diameter part 22d is prepared in the molding metal flask 20 to injection mold the sleeve for pipe joint. At least three places of ribs 23 are prepared to fix the position of the reinforced ring 6 on the outer circumference of the large diameter part 22d of this core pin 22, the sleeve is molded by pouring the resin into the molding metal flask 20 in the condition where the reinforced ring 6 is fixed beforehand in this rib 23, 23, 23 and burying the reinforced ring except for the part to contact the rib 23 in the thick part of the sleeve. COPYRIGHT: (C)2006,JPO&NCIPI
申请公布号 JP2006070993(A) 申请公布日期 2006.03.16
申请号 JP20040254989 申请日期 2004.09.01
申请人 HAJIME SANGYO KK;HITACHI METALS LTD 发明人 KAWASAKI MASAAKI;OYA HIROSHI
分类号 F16L21/00;F16L21/08;F16L33/22 主分类号 F16L21/00
代理机构 代理人
主权项
地址