A method for producing low carbon steel (13) wherein molten steel is decarburized in a three stage refining procedure comprising a first stage wherein oxygen is provided for decarburization enveloped in a gas shroud (16), a second stage wherein oxygen is provided for decarburization enveloped in a flame shroud (16), and a third stage wherein inert gas or oxygen is provided enveloped in a flame shroud (16).