摘要 |
<p>A low warp, reinforced polybutylene terephthalate molding composition includes: from about 30 weight percent to about 70 weight percent of polybutylene terephthalate resin; from about 10 weight percent to about 30 weight percent of a styrene-acrylonitrile copolymer; from about 15 to about 60 weight percent of a reinforcing agent; and optionally includes one or more impact modifiers, lubricants and stabilizers.</p> |