摘要 |
PROBLEM TO BE SOLVED: To provide a plastisol composition exhibiting excellent moldability and providing a molded product having excellent mechanical properties. SOLUTION: The plastisol composition containing polymer fine particles (P) has≤15 Pa s viscosity at 25°C at 2.6 sec<SP>-1</SP>shear rate, and provides the molded product having≥0.01 parameter I(T) represented by equation (1): I(T)=G'(T)-5×10<SP>6</SP>e<SP>-0.0189T</SP>(1) [wherein, G'(T) is a storage modulus (Pa) of the molded product obtained by molding the plastisol composition at temperature T; and the temperature T is shown by degree centigrade] within the range of 60-100°C. An molded product is obtained by molding the plastisol composition by slush molding, dip molding or rotation molding. COPYRIGHT: (C)2006,JPO&NCIPI
|