摘要 |
The use of a rechargeable lithium storage cell at a temperature lying in the range 80° C. to 180° C., said cell comprising a cathode, an anode comprising either Li<SUB>4</SUB>Ti<SUB>5</SUB>O<SUB>12 </SUB>or a carbon-containing material capable of inserting lithium, a separator, a non-aqueous solvent, and a lithium slat, wherein: the active material of said cathode is a lithiated metal oxide having the following formula: <?in-line-formulae description="In-line Formulae" end="lead"?>LiNi<SUB>1-x-y</SUB>Co<SUB>x</SUB>Al/Mn<SUB>y</SUB>O<SUB>2 </SUB><?in-line-formulae description="In-line Formulae" end="tail"?> in which: Al/Mn means Al and/or Mn; 0<=x<=0.5; 0<=y<=0.5; the sum x+y being less than 0.66; and wherein the lithium salt is selected from the group consisting of: LiPF<SUB>6</SUB>, LiBF<SUB>4</SUB>, LiBOB, LiBETI, and mixtures thereof.
|