摘要 |
1. A puncture-proof material made from at least two woven textiles connected with the use of a polymer film, where the woven textiles contain yarn with tensile strength of at least 900 Mpa, and the polymer film combining the textiles has tensile strength of at least 10 Mpa. It is characterised in that the polymer film connecting the textiles has the coefficient of elasticity from 1500 to 4500 Mpa. 8. A puncture-proof unit which contains multiple layers of the puncture-proof material, made from at least two woven textiles connected with the use of a polymer film, where the woven textiles contain yarn with tensile strength of at least 900 Mpa, and the polymer film connecting the textiles has tensile strength of at least 10 Mpa. The polymer film connecting the textiles has the coefficient of elasticity from 1500 to 4500 Mpa. 12. The application of the unit defines in claim no. 8 to produce the puncture-proof clothes.
|