发明名称 |
METHOD FOR PRODUCING RUBBER MIXTURE |
摘要 |
PROBLEM TO BE SOLVED: To provide a rubber composition which is suitable for the production of a NBR rubber suitable for producing winter tires and having devulcanization stability. SOLUTION: This method for producing a rubber mixture comprises a step for reacting a dienic elastomer, at least one light-colored reinforcing filler, and at least one polysulfide-containing alkoxysilane, and a step for mixing the obtained composition with a vulcanizing agent, at least one dithiophosphate compound and at least one vulcanization accelerator selected from sulfenamide compounds and thiazol compounds. COPYRIGHT: (C)2006,JPO&NCIPI |
申请公布号 |
JP2005336483(A) |
申请公布日期 |
2005.12.08 |
申请号 |
JP20050140671 |
申请日期 |
2005.05.13 |
申请人 |
RHEIN CHEMIE RHEINAU GMBH |
发明人 |
STEGER LOTHAR;FRUEH THOMAS;HEILIGER LUDGER |
分类号 |
B60C1/00;B29C33/02;B29C35/02;B29K9/06;B29K105/24;B29L30/00;C08K3/06;C08K3/36;C08K5/00;C08K5/47;C08K5/5398;C08K5/548;C08K9/04;C08L9/00;(IPC1-7):C08L9/00;C08K5/539 |
主分类号 |
B60C1/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|