发明名称 PROCEDIMIENTO DE FABRICACION DE LANA MINERAL, ALEGACIONES A BASE DE COBALTO PARA EL PROCEDIMIENTO Y OTRAS UTILIZACIONES.
摘要 The process for manufacturing mineral wool by internal centrifuging is characterized in that the temperature of the mineral material in the fiberizing spinner dish is at least 1150° C. and in that the fiberizing spinner dish is made of a cobalt-based alloy comprising the following elements (in percentages by weight of the alloy): the balance consisting of cobalt and inevitable impurities and the tantalum-to carbon molar ration being at least 0.3. Alloys particularly suitable for this process satisfy the above formula and do not contain tungsten. The alloys according to the invention can be used for other purposes in an oxidizing atmosphere at a temperature of at least 1100° C.
申请公布号 ES2243501(T3) 申请公布日期 2005.12.01
申请号 ES20010938312T 申请日期 2001.05.23
申请人 SAINT-GOBAIN ISOVER;SAINT-GOBAIN SEVA 发明人 BERTHOD, PATRICE;BERNARD, JEAN-LUC;LIEBAUT, CHRISTOPHE
分类号 C22F1/10;C03B37/04;C03B37/095;C22C19/07;C22F1/00;D01F9/08;(IPC1-7):C22C19/07 主分类号 C22F1/10
代理机构 代理人
主权项
地址