发明名称 Titanium alloys excellent in hydrogen absorption-resistance
摘要 A titanium alloy scarcely undergoing brittling caused by hydrogen even in case of being used under hydrogen-absorbing conditions. This alloy comprises a Ti-Al alloy composed of from 0.50 to 3.0% of Al with the balance of Ti together with unavoidable contaminants. A Ti-Al alloy material excellent in hydrogen absorption-resistance wherein an oxidized film of 1.0 to 100 nm in thickness is formed on a bulk made of a Ti-Al alloy satisfying the chemical composition as described above, and, further, a concentrated Al layer having an Al concentration of 0.8 to 25% higher by 0.3% or more than the bulk is optionally formed between the bulk and the oxidized film.
申请公布号 US2005260433(A1) 申请公布日期 2005.11.24
申请号 US20030522779 申请日期 2003.02.06
申请人 KABUSHIKI KAISHA KOBE SEIKO SHO 发明人 SAKASHITA SHINJI;YASHIKI TAKASHI;MATSUKADO KATSUHIRO;NAKAYAMA TAKENORI
分类号 C22C14/00;C23C8/10;C23C22/56;C23C26/00;C23C28/00;(IPC1-7):C22C14/00 主分类号 C22C14/00
代理机构 代理人
主权项
地址