发明名称 ABRASIVE POLISHING METHOD
摘要 The present invention is based on the practice of abrasive machining with no sealed working chamber by the employment of a visco-elastic abrasive medium, behaving predominantly as an elastic solid at the applied.strain of the orbital working motion, and applying orbital or other relative working motion to produce strain rates which bring the medium into a predominantly elastic deformation and often near, but not to exceed, the compressive stress limit at the strain rate employed. The preferred visco-elastic abrasive medium is a rheopectic poly(boro-siloxane) filled with viscosity increasing stiffening agents and high loadings of the abrasive of choice and relatively minor amounts of plasticizers. The system is operated in an open chamber under applied strain rates such that at least about 50 %, particularly about 50 to 99 %, and preferably about 80 to 95 %, of the deflection of the medium under the conditions of operation occurs by elastic deformation and is elastically recovered, and less than 50 %, particularly about 1 to 50 %, preferably about 5 to 20 %, of the deflection of the medium occurs by fluid or plastic flow.
申请公布号 CA2341737(C) 申请公布日期 2005.11.22
申请号 CA19992341737 申请日期 1999.08.25
申请人 EXTRUDE HONE CORPORATION 发明人 RHOADES, LAWRENCE J.;GILMORE, JAMES RANDALL
分类号 B24B31/116;B24B35/00;C09C1/68;C09K3/14;(IPC1-7):C09K3/14 主分类号 B24B31/116
代理机构 代理人
主权项
地址
您可能感兴趣的专利