摘要 |
PROBLEM TO BE SOLVED: To provide a decorative molded product capable of being irradiated from its backside capable of expanding the degree of freedom of a color capable of being utilized in a translucent layer and a light impervious layer while realizing a design wherein a translucent part and a light shielding part are assimilated. SOLUTION: The decorative molded product 1 capable of being irradiated from its backside is constituted by sequentially laminating the translucent layer 32 formed over the translucent part and the light shielding part adjacent to each other and the light shielding layer 34 only formed on at least one light shielding part on the surface of a molded product from a visually confirming side. When the total light transmissivity of the translucent part is set to X(%), the total light transmissivity of the light impervious part is set to Y(%) and the luminous intensity of the backside of the decorative molded product irradiated by a back light source is set to Z(lx), conditions of 2≤X≤10, 10Y≤X and Z(X-Y)≥10 are formed. COPYRIGHT: (C)2006,JPO&NCIPI
|