发明名称 LIQUID PHASE DIFFUSION JOINING METHOD FOR STEEL MEMBER WITH HOLLOW SHAPE HAVING EXCELLENT TENSILE STRENGTH AND LIQUID PHASE DIFFUSION-BONDED JOINT
摘要 PROBLEM TO BE SOLVED: To provide a liquid phase diffusion bonding method for steel members with a hollow shape applied to a machine structural component such as a cylinder, and to provide a joint. SOLUTION: In the liquid phase diffusion bonding method for steel members with a hollow shape having excellent tensile strength, steel members comprising≥0.3 mass% C, and in which at least either has a hollow shape are subjected to liquid phase diffusion bonding in such a manner that bonding foil comprising, by mass, 2.0 to 4.5% B and 0.1 to 1.0% C, and the balance Fe with impurities is used, and is melted by heating as the parts to be bonded in the steel members are pressurized and held, thereafter, the bonded parts are again heated to the temperature range from an Ac<SB>1</SB>point to (an Ac<SB>1</SB>point+an Ac<SB>3</SB>point)/2 and are held for≥3 s, so as to be subjected to liquid phase diffusion bonding. COPYRIGHT: (C)2006,JPO&NCIPI
申请公布号 JP2005288514(A) 申请公布日期 2005.10.20
申请号 JP20040109308 申请日期 2004.04.01
申请人 NIPPON STEEL CORP 发明人 SHINOHARA YASUHIRO;TSURU EIJI;ASAHI HITOSHI
分类号 B23K20/00;B23K101/06;B23K103/04;(IPC1-7):B23K20/00 主分类号 B23K20/00
代理机构 代理人
主权项
地址