摘要 PROBLEM TO BE SOLVED: To provide a Ti-based wire rod for forming molten metal in which the total content of oxygen can be sufficiently reduced though being provided with a Ti-based oxide film thicker than a naturally oxidizable film, and in its turn, the total oxygen content can easily be controlled within a standard range. SOLUTION: In the Ti-based wire rod for forming molten metal from which molten metal composed of Ti-based metal is formed by being successively heated and melted from the tip side, the wire rod body 3 is composed of Ti-based metal, and a Ti-based oxide film 2 thicker than a naturally oxidizable film is formed on the surface of the wire rod body. Regarding the total oxygen content WO<SB>T</SB>in the whole of the wire rod 3, standard upper limit value WOmax is decided. Further, in the total oxygen content WO<SB>T</SB>, the contribution to the oxygen content by the Ti-based oxide film 2 is defined as WO<SB>F</SB>, then, an upper limit regulation marginΔWO of oxygen in the body higher than the WO<SB>F</SB>is set, and the oxygen content WO<SB>M</SB>in the wire rod body 3 is regulated to WOmax-ΔWO or lower. COPYRIGHT: (C)2006,JPO&NCIPI
申请公布号 JP2005290467(A) 申请公布日期 2005.10.20
申请号 JP20040106388 申请日期 2004.03.31
申请人 DAIDO STEEL CO LTD 发明人 NAKAJOYA MAKOTO
分类号 B21C1/00;B21C9/00;C23C4/08;C23C8/10;(IPC1-7):C23C8/10 主分类号 B21C1/00
代理机构 代理人
主权项
地址