摘要 |
PROBLEM TO BE SOLVED: To provide a Taslan processed yarn having a high strength and also a good touch feeling, and a fabric by using the same. SOLUTION: This Taslan processed yarn having≥5 cN/dT strength and≥10 % elongation is obtained by using a high strength yarn consisting of≥5 pieces of filaments having 5-15 dT single fiber fineness, and having≥6 cN/dT strength and≥10 % elongation as a core yarn, and a high multi-yarn consisting of≥10 pieces of filaments having≤3 dT single fiber fineness, and having≥2 cN/dT strength and≥40 % elongation as a sheath yarn, and performing the Taslan processing. COPYRIGHT: (C)2006,JPO&NCIPI
|