发明名称 VERFAHREN FÜR AUTOTHERME REFORMIERUNG EINER KOHLENWASSERSTOFFEINSPEISUNG
摘要 An autothermal reforming catalyst consists of a zirconia support which supports ruthenium, or an inorganic oxide support which supports zirconium and ruthenium. Independent claims are also included for (A) the manufacture of an autothermal reforming catalyst by adhering solution containing ruthenium, solution containing ruthenium or cobalt or solution containing ruthenium, cobalt and magnesium to zirconia support, drying and firing, or adhering solution containing zirconium and ruthenium, solution containing zirconium, ruthenium and cobalt or solution containing zirconium, ruthenium, cobalt and magnesium to an inorganic oxide support, drying and firing; (B) the manufacture of hydrogen or synthesis gas using the catalyst; (C) catalyst for hydrocarbon reforming with carbon dioxide; (D) the manufacture of a catalyst for hydrocarbon reforming; (E) the reforming of hydrocarbons or natural gas with carbon dioxide.
申请公布号 DE69927032(D1) 申请公布日期 2005.10.06
申请号 DE1999627032 申请日期 1999.06.04
申请人 IDEMITSU KOSAN CO. LTD., TOKIO/TOKYO 发明人 FUKUNAGA, TETSUYA
分类号 B01J21/04;B01J21/06;B01J23/46;B01J23/89;B01J37/02;C01B3/38;C01B3/40 主分类号 B01J21/04
代理机构 代理人
主权项
地址