摘要 PROBLEM TO BE SOLVED: To provide a low-μpavement surface which reduces a maintenance cost. SOLUTION: This low-μpavement surface is composed of an asphalt mixture layer wherein a filler with a flow value 8-12 seconds is injected into a gap between aggregates of a pavement layer, wherein particles of pebbles are protruded from a surface of the filler by 0.3 mm or more on an average, and wherein surfaces of protruded parts of the pebbles are polished. The pavement layer is composed of an open-graded asphalt mixture wherein 55-85% pebbles with a particle diameter 13-5 mm, 5-20% pebbles with a particle diameter of 5-2.5 mm, 5-20% sand with a particle diameter of 2.5 mm - 75μm, and a 2-6% filler with a particle diameter 75μm or less, in terms of a weight ratio in the mixing of the aggregate, are contained as the aggregates. COPYRIGHT: (C)2005,JPO&NCIPI
申请公布号 JP2005240441(A) 申请公布日期 2005.09.08
申请号 JP20040052650 申请日期 2004.02.27
申请人 NIPPO CORPORATION:KK;TOYOTA MOTOR CORP 发明人 KODA MASAHIRO;KOGO KENICHI;KANEGAE TAKAHITO;OSHIKA HIROYUKI;HIKOSAKA YOSHIMASA
分类号 E01C7/18;E01C7/32;E01C7/35;(IPC1-7):E01C7/18 主分类号 E01C7/18
代理机构 代理人
主权项
地址