发明名称 FILLER FOR HEATED ASPHALT MIXTURE
摘要 <p><P>PROBLEM TO BE SOLVED: To use by-product fine powder as a filler, which can constantly satisfy a reference value of the exfoliation resistance or the like of asphalt against aggregate. <P>SOLUTION: The slaked lime content of the by-product fine powder is prepared to 3-10 mass% by using the by-product fine powder produced when the aggregates B and D are collected from a concrete lump A by grinding the concrete lump A after heating treatment is performed at 100-500°C. A specific surface area of the by-product fine powder is prepared to 5,000-10,000 cm<SP>2</SP>/g. <P>COPYRIGHT: (C)2005,JPO&NCIPI</p>
申请公布号 JP2005240343(A) 申请公布日期 2005.09.08
申请号 JP20040049294 申请日期 2004.02.25
申请人 MITSUBISHI MATERIALS CORP 发明人 TATEYASHIKI HISASHI;MIYASHIRO KAZUTOSHI;KONDO HIROSHI;YAMAZAKI MASAYASU
分类号 E01C7/22;C04B18/16;(IPC1-7):E01C7/22 主分类号 E01C7/22