发明名称 |
Method of manufacturing ink jet recording sheet |
摘要 |
A method for manufacturing ink jet recording sheet having the steps, in that order, of: providing an under-coat layer on a polyolefin coated support having the center-line average roughness of the surface of the polyolefin coated support of 0.10 to 1.5 mu m as measured at a reference length of 2.5 mm and a cutoff value of 0.8 mm; heating the polyolefin coated support on which the under-coat layer is provided; and coating on the under-coat layer a coating liquid that contains inorganic micro particles and binder so that the coating liquid forms a porous ink absorption layer, wherein the temperature difference between the temperature of the polyolefin coated support and the temperature of the coating liquid is within 15 DEG C in the coating step.
|
申请公布号 |
EP1571004(A1) |
申请公布日期 |
2005.09.07 |
申请号 |
EP20050251241 |
申请日期 |
2005.03.02 |
申请人 |
KONICA MINOLTA PHOTO IMAGING, INC. |
发明人 |
SUZUKI, SHINICHI;OHBAYASHI, KEIJI |
分类号 |
B41M5/00;B41M5/50;B41M5/52;D21H27/00;(IPC1-7):B41M5/00 |
主分类号 |
B41M5/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|