发明名称 |
Metal alloys for forming conductive oxide coatings for electrical contacts |
摘要 |
Described is a metal alloy comprising at least two metal elements which are not precious metals, said alloy being capable of forming a surface metal oxide layer that is conductive having a contact resistivity of 100 Omegacm or less after the alloy has been subjected to 125° C. for 1008 hours. Also described is a process of preparing a metal alloy providing two metal elements which are not precious metals and oxidizing the metal alloy to produce a surface metal oxide layer that is conductive having a contact resistivity of 100 Omega-cm or less after the alloy has been subjected to 125° C. for 1008 hours. |
申请公布号 |
US2005189041(A1) |
申请公布日期 |
2005.09.01 |
申请号 |
US20050039579 |
申请日期 |
2005.01.20 |
申请人 |
MANTESE JOSEPH V.;EDDY DAVID S.;AUKLAND NEIL R.;THOMPSON MARGARITA P.;WANG SU-CHEE S. |
发明人 |
MANTESE JOSEPH V.;EDDY DAVID S.;AUKLAND NEIL R.;THOMPSON MARGARITA P.;WANG SU-CHEE S. |
分类号 |
C22C9/00;C23C8/10;(IPC1-7):C22C9/00 |
主分类号 |
C22C9/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|