摘要 |
In a method for producing a metal/ceramic bonding member wherein an electroless nickel alloy plating layer 18 is formed on a predetermined portion of the surface of an aluminum plate 12 which is bonded to at least one side of a ceramic substrate 10 and which is formed so as to have a predetermined circuit pattern, an alkali peeling type resist 16 having a predetermined shape is applied on the surface of the aluminum plate 12 before forming the electroless nickel alloy plating layer 18 , and then, a portion of the surface of the aluminum plate 12 , on which the resist 16 is not applied, is activated with an acidic zinc immersion solution containing a fluoride or silicofluoride. Then, after the electroless nickel alloy plating layer 18 is formed, the resist 16 is removed with an alkali.
|