摘要 |
A magnetic storage device has a magnetic layer, the magnetic crystal grains of which are separated by a nonmagnetic phase. The typical crystal grain is in the approximate shape of a sphere or an ellipsoid. The thickness of the magnetic crystal grains, which is in the direction perpendicular to the surface or the film, is smaller than that of the thickness of the magnetic film. The ratio of the coercive force, which is measured in the circumferential direction, to the coercive force, which is measured in the radial direction, (the orientation ratio of the coercive force), is larger than 1.0, but preferably nor greater than 3.0. Further, the area fraction of the magnetic grains having an extended axis within 30° from the circumferential direction is equal to or more than 45%.
|