摘要 |
PROBLEM TO BE SOLVED: To provide a coating method which enables the sufficient coating of microspikes. SOLUTION: The method consists of a process of applying an electrodeposition coating on a coating surface 1 containing a minute protrusion 1a to form an electrodeposition coating layer 2, a process of applying a rustpreventive paint where polyester-melamine-epoxy base resin containing a rustpreventive pigment is a substrate, on the surface of the electrodeposition coating layer 2 to form a rustpreventive coating layer 3, a process of applying a top coat on the surface of the rustpreventive coating layer 3 to form a top coating layer 4, and a hardening process of hardening simultaneously the electrodeposition coating layer 2, the rustpreventive coating layer 3, and the top coating layer 4. COPYRIGHT: (C)2005,JPO&NCIPI
|