发明名称 METHOD FOR RECONSTRUCTING A BITUMINOUS-SURFACED PAVEMENT
摘要 <p>A method of reconstructing a bituminous-surfaced pavement is provided. This method includes evaluating the pavement to determine if it is an appropriate candidate for full-depth reclamation; mixing an emulsion with reclaimed asphalt pavement particles from the pavement to form an asphalt emulsion mix; and testing the asphalt emulsion mix for performance using a cohesion test, a moisture susceptibility test, and a modulus test. In many instances, dirt and/or aggregate form the base layer of the pavement are also included in the asphalt emulsion mix. The invention also includes designing a full-depth reclamation (FDR) layer based on this test data. Once the layer is designed, the bituminous surface of the pavement is pulverized, an emulsion is mixed with the pulverized reclaimed asphalt pavement particles from the bituminous surface and possibly dirt and/or aggregate form beneath the bituminous surface of the pavement, and this mixture is applied to the pavement.</p>
申请公布号 WO2005066418(A1) 申请公布日期 2005.07.21
申请号 WO2004US38551 申请日期 2004.11.17
申请人 KMC ENTERPRISES, INC.;GRUBBA, BILL;THOMAS, TODD 发明人 GRUBBA, BILL;THOMAS, TODD
分类号 G01M99/00;C08L95/00;E01C11/00;E01C23/06;(IPC1-7):E01C23/06 主分类号 G01M99/00
代理机构 代理人
主权项
地址