发明名称 RUBBER COMPOSITION FOR VIBRATION ISOLATION
摘要 PROBLEM TO BE SOLVED: To provide a rubber composition for vibration isolation, having excellent vibration isolation performance giving stable tanδover a wide temperature region from low temperatures to high temperatures. SOLUTION: This rubber composition for vibration isolation is obtained by blending 100 pts.mass of a polymer (A) having a glass transition temperature (Tg) in the range of -80 to 0°C, a solubility parameter (SP value) in the range of 7.5-8.5, 5-150 pts.mass of a polymer (B) having a glass transition temperature (Tg) in the range of 10-60°C, a solubility parameter (SP value) of≥8.5 and 5-50 pts.mass of a polymer (C) having a melting point (Tm) in the range of 50-160°C, a solubility parameter (SP value) of≥8.5 as essential components. Preferably, tanδof the rubber composition for vibration isolation is≥0.4 in the range of temperature of -30 to 60°C. COPYRIGHT: (C)2005,JPO&NCIPI
申请公布号 JP2005179525(A) 申请公布日期 2005.07.07
申请号 JP20030422992 申请日期 2003.12.19
申请人 YAMAUCHI CORP 发明人 MARUKO HIROYUKI;KIDO KENICHIRO
分类号 F16F15/08;C08L101/00;C09K3/00;(IPC1-7):C08L101/00 主分类号 F16F15/08
代理机构 代理人
主权项
地址