摘要 |
PROBLEM TO BE SOLVED: To enable increase of yield by restraining fusion welding of a component which is used at the time of sintering to a magneto compact. SOLUTION: In a method for manufacturing a rare earth sintered magnet wherein the magneto compact containing rare earth elements is sintered, the magneto compact is sintered in the state that the magneto compacts are laminated through the board of a mesh type. Alternatively, the magneto compact is sintered in the state that the magneto compact is wrapped with a metal foil and the board of a mesh type is interposed between the metal foil and the magneto compact. Since the board of a mesh type has a small contact area with the magneto compact and is hardly adhered, fusion welding to the magneto compact is restrained even in a case that the magneto compacts are laminated and sintered. COPYRIGHT: (C)2005,JPO&NCIPI
|