摘要 |
PROBLEM TO BE SOLVED: To provide a laminated ceramic electronic component capable of preventing internal defects at baking and occurrence of cracks due to an external shock. SOLUTION: The laminated ceramic electronic component is configured such that internal electrodes 3, 4 are laminated with each of a plurality of first dielectric layers 2a inbetween to form a laminated body 1, a first dielectric layer 2b is coated and formed to both principal sides of the laminated body 1, and external electrodes 5, 6 electrically connected to the internal electrodes 3, 4 are coated and formed to end faces of the laminated body 1. The void rate of the first and second dielectric layers 2a, 2b is selected as 0.01% to 1.00%, and the void rate of the first dielectric layer 2a is higher than the void rate of the display second dielectric layer 2b. COPYRIGHT: (C)2005,JPO&NCIPI
|