摘要 |
FIELD: electric luminescent light sources. ^ SUBSTANCE: at least two non-transparent electrodes are applied to dielectric substrate, which electrodes are positioned in same plane with space relatively to each other. Continuous dielectric layer is applied to electrodes, on top of which continuous layer of electro-phosphor is formed in linking agent. On top of said layer of phosphor in linking agent transparent electrode is applied in form of layer of dispersion tin oxide, containing 0.2-1.1 percents of mass of antimony, received by processing tin oxide serially by fumes of antimony chloride and water at 140 - 180°C with following baking in the air at 700-900° in linking agent at relation (80-20) - (20-80) percents of mass, while as said linking agent butadiene-nitrile rubber. On top of said at least two electrodes polymer layer can be additionally applied, including low-dispersion carbon in butadiene-nitrile rubber. ^ EFFECT: higher stability, higher reliability. ^ 2 cl, 3 dwg, 1 tbl, 10 ex |