摘要 The invention relates to a process for the manufacture of a shaped part of ultra high molecular weight polyethylene (UHMW-PE) comprising melt processing, wherein UHMW-PE a) is annealed at a temperature between 130° C. and 136° C., preferably at about 135° C. for at least one hour, b) is converted into a shaped part at a temperature above 142° C.; and c) is cooled down to a temperature below 135° C. The inventiion further relates to a part like a fibre made with the process and the use of the fibre in a bio medical application.
申请公布号 US2005121825(A1) 申请公布日期 2005.06.09
申请号 US20040493836 申请日期 2004.12.13
申请人 RASTOGI SANJAY;KURELEC LADA 发明人 RASTOGI SANJAY;KURELEC LADA
分类号 B29B13/02;B29C67/24;B29K23/00;D01F6/04;(IPC1-7):B29C71/02;B29C55/04;B29C55/12 主分类号 B29B13/02