摘要 |
PROBLEM TO BE SOLVED: To obtain a luminescent pigment which emits a silky, deep, subdued, delicate glitter (silky looking) and a manufacturing method whereby the luminescent pigment can be manufactured. SOLUTION: The luminescent pigment has a structure wherein thin films 1 of flaky titanic acid are laminated. The space between the flaky titanic acid thin films can be left as a void 2 or filled with a polymeric resin 4, and the surface of the flaky titanic acid thin film 1 can be covered with the polymeric resin 4. The luminescent pigment can be obtained by forming a coating film from a coating material wherein the flaky titanic acid is dispersed in a polymeric resin solution and pulverizing the coating film. COPYRIGHT: (C)2005,JPO&NCIPI
|