摘要 |
A racket frame including a first laminate composed of a plurality of first prepregs consisting of fiber reinforced resin and a second prepreg, consisting of fiber reinforced resin, which is layered on the first laminate. The first laminate has a loss factor (=tan delta) set to not less than 0.005 nor more than 0.02, when the loss factor is measured at a temperature of 10° C. and a frequency of 10 Hz. The second prepreg has a loss factor (=tan delta) set to not less than 0.10 nor more than 0.50, when the loss factor is measured at a temperature of 10° C. and a frequency of 10 Hz.
|