发明名称 ADMIXTURE FOR SOIL PAVEMENT AND SOIL PAVEMENT USING THE SAME
摘要 PROBLEM TO BE SOLVED: To provide an admixture, which is incorporated in a soil pavement and adds resistance to mud and cracking resistance to the soil pavement while maintaining sufficient strength. SOLUTION: The admixture for a soil pavement contains 100 pts.wt. of a polyvinyl alcohol polymer with the saponification degree of 80-99% and the polymerization degree of 50-4,000 and 30-240 pts.wt. of one or a plurality of plasters selected from the type II of anhydrous plasters, the type III of anhydrous plasters, dihydrate gypsum and hemihydrate gypsum. The admixture also contains 10-300 pts.wt. of a hydraulic material to 100 pts.wt. of the polyvinyl alcohol polymer, and further contains 1-20 pts.wt. of amorphous silica to 100 pts.wt. of the admixture for the soil pavement. COPYRIGHT: (C)2005,JPO&NCIPI
申请公布号 JP2005133064(A) 申请公布日期 2005.05.26
申请号 JP20040213721 申请日期 2004.07.22
申请人 DENKI KAGAKU KOGYO KK 发明人 HIGUCHI TAKAYUKI;ANDO TETSUYA;WATANABE SATOSHI
分类号 E01C7/36;C09K17/02;C09K17/06;C09K17/20;C09K17/40;C09K103/00;(IPC1-7):C09K17/40 主分类号 E01C7/36
代理机构 代理人
主权项
地址