发明名称 ОГНЕУПОРНЫЙ ВСПЕНЕННЫЙ УГЛЕРОДСОДЕРЖАЩИЙ КОМПОЗИЦИОННЫЙ МАТЕРИАЛ
摘要 FIELD: building and refractory materials. ^ SUBSTANCE: invention relates to manufacturing light porous carbon-containing refractory materials. Invention proposes material showing inorganic cellular structure prepared by foaming and hardening the slip composition prepared from ground charge with a gas-forming agent - finely divided crystalline silicon mixed with water glass in the following mass ratios of components in the slip composition: water glass : silicon = (3-6):1 and charge : water glass = (1.0-1.5):1. Charge comprises components in the following ratio, mas. p. p.: mineral filling agent, 45-53; calcined shungite, 15-22; aluminum powder, 10-15. Quartz sand, quartzite, perlite, vermiculite, dinas, cement fly ash and slags are used as a mineral filling agent, Foamed material comprises 12-20 wt.-% of silicon carbide and 25-51 wt.-% of kyanite prepared by exothermic reaction at 1400-1700°C carrying out in volume of hardened porous material. Material shows porosity 60-81% and heat conductivity 0.08-0.18 Wt/m x K at 20°C and shows high mechanical indices and stability in oxidizing medium. Material can be prepared without large energy and labor consumptions. ^ EFFECT: improved and valuable properties of material. ^ 2 cl, 1 tbl
申请公布号 RU2003136383(A) 申请公布日期 2005.05.20
申请号 RU20030136383 申请日期 2003.12.17
申请人 Закрытое Акционерное Общество Научно-производственно-Коммерческа  фирма "МаВР" (ЗАО НПКФ "МаВР") (RU) 发明人 Карпухин Игорь Алексеевич (RU);Мойзис Сергей Евгеньевич (RU);Владимиров Владимир Сергеевич (RU);Илюхин Михаил Анатольевич (RU);Мойзис Евгений Сергеевич (RU);Рыбаков Сергей Юрьевич (RU)
分类号 C04B38/02;C04B35/16;C04B38/10 主分类号 C04B38/02
代理机构 代理人
主权项
地址