发明名称 СПОСОБ И КОМПОЗИЦИЯ ДЛЯ ДЕВУЛКАНИЗАЦИИ ОТРАБОТАННОЙ РЕЗИНЫ
摘要 Mechanical/chemical method and composition for de-vulcanization of rubber maintains the macromolecules, renders sulfur passive for later re-vulcanization, is cost effective, environmentally friendly and produces high quality de-vulcanized rubber to replace virgin rubber. Waste rubber is shredded, crushed and metal-removed. Modifying composition is added as the particles of shredded waste rubber are poured between two rollers that further crush the particles. The modifying composition is a mixture of (1) a proton donor that selectively breaks the sulfur bonds and renders the sulfur passive, (2) a metal oxide and (3) an organic acid that build new bonds between macromolecules for later re-vulcanization, (4) an inhibitor that prevents re-attachment of sulfur radicals with each other before the proton donor attaches itself to the sulfur and (5) a friction agent that prevents sliding of the waste rubber between the rollers. The particles are subjected to at least ten sets of rollers.
申请公布号 RU2003136615(A) 申请公布日期 2005.05.20
申请号 RU20030136615 申请日期 2002.05.20
申请人 ЭКСЕР ХОЛДИНГ КОРПОРЕЙШН (US) 发明人 ГОЛДШТЕЙН Вадим (IL);КОПИЛОВ Михаил (IL)
分类号 B29B17/02;B29B17/04;B29K21/00;C08J11/04;C08J11/10;C08J11/18 主分类号 B29B17/02
代理机构 代理人
主权项
地址