摘要 PROBLEM TO BE SOLVED: To obtain an FRP molded body excellent in strength and precision with an excellent yield by using a laminated film at the time of manufacture of the FRP molded body. SOLUTION: Heat shrinkage factors in directions of length and width in the case when the thickness is 15-30μm and exposure is made for 15 minutes in a temperature range of 80-100 deg.C are in a range of -0.5-1.0% respectively and the heat shrinkage factors in the directions of length and width in the case when the exposure is made for 15 minutes in a temperature range of 120-130 deg.C are in a range of 0.5-3.0% respectively, while the elongation under a load of 6.0-6.7 kg/mm<2> is within 10%.