摘要 |
Yield, particularly when treating hardwood chips, can be improved by at least 1-2% in a kraft cellulose pulping process by keeping the temperature and effective alkali (EA) low during impregnation, and by keeping the EA low in at least a first cook stage. After cooking, the pulp is subjected to cooling low EA liquor, e.g. to reduce its temperature to below 120° C. (preferably below 100° C.) with an EA below about 5 g/L (expressed as NaOH). Continuous treatment in a continuous digester system is preferred, with the EA below about 20 g/L during impregnation and the first cook.
|