发明名称 |
Process for making nano-sized and sub-micron-sized lithium-transition metal oxides |
摘要 |
A process is provided for making nano-sized or sub-micron sized oxides of lithium and a transition metal. The desired size is generally in the range 10 nm to 1000 nm and preferably in the range 10 nm to 100 nm. The particles have a narrow size distribution. The process includes milling and re-firing under controlled conditions so that crystallites of the desired particle size are grown.
|