发明名称 SURFACE CONDITIONING METHOD FOR CONTINUOUSLY CAST SLAB
摘要 PROBLEM TO BE SOLVED: To provide a surface conditioning method for a continuously cast slab which completes the work efficiently by distinguishing the necessity and area to be conditioned in advance when the surface conditioning is performed on the cast slab prior to charging it into a heating furnace. SOLUTION: The continuously cast slab is hot-scarfed on its surface, then charged into the heating furnace, and sent to the rolling process after removal of oxide scale generated in the heating furnace. Based on a detection result of the cast slab surface irregularity after hot scarfing and the heating furnace conditions to affect the oxide scale thickness formed during heating, the cast piece surface irregularity after the removal of oxide scale is estimated. If the estimated irregularity exceeds a predetermined threshold value, the irregularity on the cast slab surface is removed before the cast slab is sent to the heating furnace. COPYRIGHT: (C)2005,JPO&NCIPI
申请公布号 JP2005074496(A) 申请公布日期 2005.03.24
申请号 JP20030309774 申请日期 2003.09.02
申请人 KOBE STEEL LTD 发明人 KOKITA MASAHIKO
分类号 B22D31/00;B23K7/06;(IPC1-7):B22D31/00 主分类号 B22D31/00
代理机构 代理人
主权项
地址