摘要 |
PROBLEM TO BE SOLVED: To provide a fiber-reinforced crystalline thermoplastic resin composition, scarcely causing decrease in mechanical strengths and excellent in an external appearance of a molded product therefrom, and to provide pellets of the same. SOLUTION: This composition contains a resin (I) which contains a crystalline thermoplastic resin (a component (A)) in an amount of 10-99 wt% and a crystalline thermoplastic resin (a component (B)) having a crystallization temperature lower than that of the component (A) by not less than 10°C in an amount of 10-1 wt%, and further contains a fiber (a component (C)) in an amount of 5-400 pts.wt. based on 100 pts.wt. of the resin (I). The pellets are obtained from the composition. The molded product is obtained from the composition or the pellets. COPYRIGHT: (C)2005,JPO&NCIPI
|