发明名称 |
Iron based alloy material for thixocasting process and method for casting the same |
摘要 |
An iron based alloy material for a thixocasting process and a method for casting the material which extends the service life of dies by inhibiting solidification contraction, and in which casting defects such as size variations and cracks can be inhibited. The material comprises 1.6 wt %<=C<=2.5 wt % and 3.0 wt %<Si<=5.5 wt %, and a carbon equivalent (the value of CE) defined as "C(wt %)+1/3Si(wt %)" of 2.9 to 3.5. This material is made to be in a half-melted state with 35 to 50 wt % of a solid phase to be cast under a pressure load.
|
申请公布号 |
US6863744(B2) |
申请公布日期 |
2005.03.08 |
申请号 |
US20020235855 |
申请日期 |
2002.09.06 |
申请人 |
HONDA GIKEN KOGYO KABUSHIKI KAISHA |
发明人 |
TSUCHIYA MASAYUKI;UENO HIROAKI |
分类号 |
B22D18/02;B22D17/00;C22C1/00;C22C33/08;C22C37/06;C22C37/10;C22C38/00;C22C38/02;C22C38/36;(IPC1-7):C22C38/02;C22C38/34 |
主分类号 |
B22D18/02 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|