<p>The invention lies in that an alloy of Al and two or more of Ca, Mg and REM is added as a deoxidizing agent to molten steel and Al2O3 in the resulting inclusion is adjusted to a range of 30-85 wt% to obtain alumina cluster-free Al-killed steel.</p> |