摘要 |
<p>Process for obtaining zeolitic bodies consisting of at least 95 % by weight zeolite LSX, comprises the following operations: agglomeration of zeolite LSX powder with a binder containing at least 80 % by weight of a clay able to undergo zeolitization, forming of the obtained mixture, drying and calcining at a temperature of 500 °C to 600 °C, contacting of the product resulting from previous step with aqueous caustic solution and washing, drying and activation at a temperature of 500 °C to 600 °C.</p> |