发明名称 GLASS COMPOSITION, MIXTURE, PASTE, GREEN SHEET AND PLASMA DISPLAY PANEL
摘要 PROBLEM TO BE SOLVED: To provide a lead-free glass worked at a temperature lower than 550°C, having a desired thermal expansion coefficient and exhibiting high water resistance. SOLUTION: As glass components, 35 to 45 mole % of P<SB>2</SB>O<SB>5</SB>, 45 to 55 mole % of ZnO, and 5 to 15 mole % of one or more of alkaline earth metal oxides selected from the group consisting of CaO, SrO and BaO are contained. COPYRIGHT: (C)2005,JPO&NCIPI
申请公布号 JP2005022961(A) 申请公布日期 2005.01.27
申请号 JP20040171778 申请日期 2004.06.09
申请人 MITSUBISHI MATERIALS CORP 发明人 KUROMITSU YOSHIO;UESUGI RYUJI;SUGAMURA KUNIO;TOYODA SEIJI;FUJINO SHIGERU;TAKEBE HIROMICHI
分类号 C03C3/16;C03C3/074;H01J11/22;H01J11/34;H01J11/36;H01J11/38;(IPC1-7):C03C3/16;H01J11/02 主分类号 C03C3/16