发明名称 |
High mineral oil content styrene polymers used e.g. in moldings, films or foams are obtained by screw extrusion mixing with mixers or kneaders at the oil introduction zones |
摘要 |
<p>Production of styrene polymers with a mineral oil content >= 8 wt.% by mixing comprises: (a) using an extruder with one or more screws; and (b) introducing the mineral oil at >= 2 openings, there being mixing or kneading elements in the vicinity of the openings.</p> |