发明名称 FREE-CUTTING STEEL
摘要 A low carbon free cutting steel can be obtained by allowing the steel to contain 0.02 to 0.15 mass % of C, 0.05 to 1.8 mass % of Mn, 0.20 to 0.49 mass % of S, more than 0.01 mass % and not more than 0.03 mass % of O 0.3 to 2.3% of Cr, and the balance consisting of Fe and inevitable impurities, the Cr/S ratio falling within a range of between 2 and 6. <IMAGE>
申请公布号 EP1449932(A4) 申请公布日期 2005.01.26
申请号 EP20020783714 申请日期 2002.11.29
申请人 NKK BARS & SHAPES CO., LTD.;NATIONAL INSTITUTE OF ADVANCED INDUSTRIAL SCIENCE AND TECHNOLOGY;ISHIDA, KIYOHITO 发明人 ISHIDA, KIYOHITO;MURAKAMI, TOSHIYUKI;SHIRAGA, TETSUO;OIKAWA, KATSUNARI
分类号 C22C38/00;C22C38/04;C22C38/18;C22C38/58;C22C38/60 主分类号 C22C38/00