摘要 |
PROBLEM TO BE SOLVED: To provide a corrosion resistant alloy which has excellent corrosion resistance to a smelt, and can eliminate increase in the production cost caused by cracks or the like, to provide a corrosion resistant member, and to provide a production method therefor. SOLUTION: At least a part of the surface 13a' of the corrosion resistant member is covered with a corrosion resistant alloy 13b consisting of an Al-Cr-Ni based alloy comprising Al in the range of 3 to 10 wt.%. COPYRIGHT: (C)2005,JPO&NCIPI
|